COLD WORK TOOL STEEL D2
COLD WORK TOOL STEEL D2
Cold Work D2 tool steel is a high carbon, high chromium device steel (12% chrome) with amazingly high wear opposing properties, heat treatable to 60-62 Rc.
D2 steel is extremely wear safe yet not as intense as lower alloyed steels. D2 tool steel solidifies in air with a low request of development and offers a measure of erosion resistance when cleaned.
The high percentage of chromium gives it mild corrosion-resisting properties in the hardened condition.The mechanical properties of D2 are exceptionally sensitive to heat treatment. D2 steel is accessible in de-carb free adjusts, pads, and squares, and also ground flat stock and drill rod.
Element | Min | Max |
---|---|---|
Carbon, C | 1.55 | 1.75 |
Manganese, Mn | 0.20 | 0.40 |
Silicon, Si | 0.25 | 0.40 |
Molybdenum, Mo | 0.50 | 0.70 |
Chromium,Cr | 11.00 | 12.00 |
W | 0.40 | 0.60 |
Vanadium, V | 0.10 | 0.50 |
Co | -- | -- |
Properties | Metric | Imperial |
---|---|---|
Density | 7.7 x 1000 kg/m3 | 0.278 lb/in3 |
Melting point | 1421°C | 2590°F |
Mechanical Properties | Metric | Imperial |
---|---|---|
Hardness, Knoop (converted from Rockwell C hardness) | 769 | 769 |
Hardness, Rockwell C | 62 | 62 |
Hardness, Vickers | 748 | 748 |
Izod impact unnotched | 77.0 J | 56.8 ft-lb |
Poisson's ratio | 0.27-0.30 | 0.27-0.30 |
Elastic modulus | 190-210 GPa | 27557-30457 ksi |
Properties | Conditions | ||
---|---|---|---|
T (°C) | Treatment | ||
Thermal expansion | 10.4 x 10 -6 /ºC | 20-100 | - |
Heat Treatment
Forging
Annealing
Martempering
Final Grinding
Hardening
Stress Relieving